TECHNET Archives

June 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wbsx4-000BjMC; Wed, 11 Jun 97 14:21 CDT
Old-Return-Path:
Date:
Wed, 11 Jun 1997 15:31:14 -0400 (EDT)
>From willli Wed Jun 11 14:
21:28 1997
Precedence:
list
X-Loop:
Message-ID:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/13317
From [log in to unmask] Tue Jun 17 10:
48:02 1997
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"UJ2fc1.0.H-K.Tgldp"@ipc>
Subject:
From:
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
Parts/Attachments:
text/plain (18 lines)
Not many shops carry G10 as most of the work being done
needs to be UL approved and G10 doesn't cut it.  In fact, it
may be difficult to get the old stuff now anyway.  When the 
bromine was added years ago, it made plated thru holes
very difficult until people realized the change and chemical
changes of  the deposition process had to be made.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2