X400-Content-Type: |
P2-1988 ( 22 ) |
Old-Return-Path: |
|
Date: |
11 Jun 1997 09:48:42 -0500 |
X-Loop: |
|
Precedence: |
list |
Resent-From: |
|
Conversion: |
Allowed |
Disclose-Recipients: |
Prohibited |
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
Priority: |
normal |
X-Mailing-List: |
|
X400-Originator: |
|
Content-Return: |
Allowed |
X400-MTS-Identifier: |
[/c=US/admd=MCI/prmd=Honeywell/; 04068339EBACA006-HW-MTA-AZ] |
TO: |
|
>From willli Wed Jun 11 09: |
38:53 1997 |
Return-Path: |
<TechNet-request> |
Alternate-Recipient: |
Allowed |
X400-Recipients: |
non-disclosure; |
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0wboXo-000BjGC; Wed, 11 Jun 97 09:38 CDT |
Message-Id: |
<04068339EBACA006*/c=US/admd=MCI/prmd=Honeywell/o=AZ-MTA/ou=MSMail/ou=IAC/s=Lolmaugh/g=Scott/@MHS> |
Resent-Message-ID: |
<"Z3K6U2.0.oD1.fXhdp"@ipc> |
Subject: |
|
From: |
|
From [log in to unmask] Tue Jun 17 10: |
44:37 1997 |
X400-Received: |
by mta HW-MTA-AZ in /c=US/admd=MCI/prmd=Honeywell/; Relayed;
11 Jun 1997 09:48:42 -0500
by /c=US/admd=MCI/prmd=Honeywell/; Relayed;
11 Jun 1997 09:48:42 -0500 |
Original-Encoded-Information-Types: |
IA5-Text |
Content-Identifier: |
04068339EBACA006 |
Parts/Attachments: |
|
|
All,
Beware plugging vias that have solder inside them. No matter how good the
plugging and overlying soldermask job, during reflow the underlying solder
will expand as it heats. When the solder hits liquidous, the pressurized
fluid can force a jet of molten solder through any point of thin coverage
due to misregistration or pinholes, leaving either solder balls or solder
strings . I have seen microscopic "wires" of solder that have been extruded
through pinholes as the pressure of the molten solder forces it out. These
strings can be longer than 0.100" and are virtually invisible to the naked
eye. If you must plug vias, do it in direct contact with the base metal.
----------
From: [log in to unmask]
To: [log in to unmask]
Subject: via plugging
Date: Wednesday, June 11, 1997 7:46AM
I'd recommend you fill them with solder if you can. Coating can be used,
but
its best if you do this AFTER a protective coating is applied to the board
like
Hot Air Solder Level (hasl) or on a patern plated board (SnPb plated) from
which you DO NOT strip the Sn Pb .
See my other append about solutions getting trapped in the vias.
If at all Possible DO NOT Plug/Tent/Fill vias with anything other than a
solder
like material that fills them 100% of their depth.
hope that helps
Jim Herard
IBM Microelectronics
Quality Engineering
[log in to unmask]
---------------------- Forwarded by Jim Herard/Endicott/IBM on 06-11-97
08:39
AM
---------------------------
suixin @ elis.rug.ac.be
06-10-97 03:59 PM
Please respond to [log in to unmask] @ internet
To: TechNet @ ipc.org @ internet
cc:
Subject: via plugging
Hello, everybody
I want to get some information on via plugging technology. In my
work, the plated through vias are 1.6mm deep and 300 micron in
diameter. I have to plug them before further processing. Any input
will be greatly appreciated.
Thanks in advance.
suixin zhang
ELIS-TFCG/IMEC, University of Ghent
Sint-Pietersnieuwstraat 41, B-9000 Ghent, Belgium
tel: 0032-9-2643371
fax: 0032-9-2643594
Email: [log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|