Michael,

We do a great deal of PCB evaluations and can provide most, if not all, of the work you're looking for. Please contact me offline if you'd like. 
Paul Terranova
[log in to unmask]
Phone: 508-467-3109
FAX: 508-467-6796

DIGITAL's Analytical and Environmental Test Services Lab
Digital Equipment Corporation
M/S: MRO1-3/D2
200 Forest Street  
Marlboro, MA  01752



From:	Michael Forrester [SMTP:[log in to unmask]]
Sent:	Thursday, May 22, 1997 5:25 PM
To:	[log in to unmask]
Subject:	PCB Testing House

Does anyone know of a good PCB testing house?  We plan to create a test board using various packages and various copper protective finishes.  I need to send the boards to a testing facility to test various parameters such as, peel strength, solderability, microsectional analysis od solder joints, and interconnection reliability using thermal cycling and vibration.
Best Regards,
Mike Forrester
[log in to unmask]

***************************************************************************

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************