Has anyone experienced dull, dark gray SMT solder joints after cleaning?
I am using a dishwasher and a neutralizer could these be the problems??
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Dan Sadley
[log in to unmask]
3660 Quakerbridge rd.
Trenton, NJ 08619
(609) 587-9897 x-179
Fax (609) 587-1970
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
***************************************************************************