Hi all,
Does any one have any suggestions for a solder type to attach Elkonite to
aluminum? My primary concern is the CTE differences; this is for an
assembly that sees temps from -65C to almost 200C ... thanks for any thoughts!
Sheila Smith, Tracor AES
***************************************************************************