2113 is used a lot in Europe where it more or less replaces 2125 as a 4 mil
prepreg. It presses maybe a smidgeon thinner but not much (depending on the
resin content favoured by your local supplier). The only downside is that it
has almost the same thread count as 2116 and is therefore difficult to
distinguish visually. this can lead to confusion and the odd mistake among
companies that employ humans.
Dave Heywood
[log in to unmask]
----------
From: [log in to unmask]
To: [log in to unmask]; Dave Heywood
Subject: Re:FAB Prepreg style 2113
Date: 21 May 1997 03:08
<<File Attachment: ENVELOPE.TXT>>
We are after typical build uses of style 2113 prepreg.
Any help would be appreciated.
Regards,
David Taylor
Chief Engineer
East Coast Printed Circuits
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************