I would like to find out more about Permanganate desmearing.
What are the bath make-ups (ie. components and concentrations),
process parameters (i.e.. time and temperatures) used for epoxy type
boards.
What are the positive and negative aspects for these materials or
operations?
Are there any good (safe) chemistries other than permanganates for
epoxies, acrylics or polyesters?
Thanks in advance. You can answer me through technet or personally at
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
----------
Received: from sol.corp.harris.com by post.fabrik.com
with SMTP (Fabrik F07.0-000)
id [log in to unmask] ; Sat, 17 May 1997 03:34:10 -0700
Received: from mailc.harris.com by sol.corp.Harris.COM (8.6.12/ Harris.COM Unix
mail relay)
id GAA08064; Sat, 17 May 1997 06:34:05 -0400
Received: from ccMail by mailc.harris.com
(IMA Internet Exchange 2.1 Enterprise) id 000495B3; Sat, 17 May 97 06:35:52
-0400
Mime-Version: 1.0
Date: Sat, 17 May 1997 06:34:03 -0400
Message-ID: <[log in to unmask]>
From: [log in to unmask] (Administrator)
Subject: Message not deliverable
To: "Duane B. Mahnke" <[log in to unmask]>
Content-Type: text/plain; charset=US-ASCII
Content-Transfer-Encoding: 7bit
Content-Description: cc:Mail note part
----------
---------------------------- Forwarded with Changes ---------------------------
From: "Administrator" <[log in to unmask]> at
-FABRIK/Internet
Date: 5/17/97 3:34AM -0700
To: Duane B. Mahnke at Rogers-MCD
Subject: Message not deliverable
-------------------------------------------------------------------------------
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|