     Hello Tamir:
     
     The electrical conductivity of Pd is 0.0950 x10+6 ohm-1 cm-1 at 20C.
     
     
     Dave Hillman
     Rockwell Collins
     [log in to unmask]


______________________________ Reply Separator _________________________________
Subject: Pd edge connectors
Author:  [log in to unmask] at ccmgw1
Date:    5/13/97 8:19 AM


     Hello,
     
     1. I need some information about the Pd coating on the edge connector 
     
        instead of the common chemical Ni-Au.
     
     2. Does any one know the conductivity of Pd.
     
     Thanks, Tamir
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2