> I have just recently been put in charge of routing and blanking and I am
> encountering several issues. Do most of you out there let/have operators
> that change the compensations? Do you have to change them frequently and
> over and over again on the same P/N's? Is there software that can help
with
> fabrication?
>
> The reasons for my questions is that we have arrays on panels that on one
> side of the panels is fine, but on the other end we start cutting into
the
> fingers. We also have arrays with 3 boards and on the outside cut the
board
> is 0.020" to wide and the 2 internal boards they are 0.018" to short.
Most
> of the problems seem to be that when we move away from on edge of the
panel
> during routing that the dimensions of the routed boards and arrays
worsen.
> It seem that this has to be compensation because material does not move
> that symmetrical.
>
> Any help would be appreciated.
>
>
***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05
*
>
***************************************************************************
> * To subscribe/unsubscribe send a message <to: [log in to unmask]>
*
> * with <subject: subscribe/unsubscribe> and no text in the body.
*
>
***************************************************************************
> * If you are having a problem with the IPC TechNet forum please contact
*
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]
*
>
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|