Tamir,
Try the March 1997 issue of SMT Magazine as well as back issues of
Printed Circuit Fabrication Magazine. I have also found good
information at the Merix Corporation web site on DYCOstrate Technology
and Plasma etched redistribution layers.
http://www.merix.com/ps/micro_wp.html
- David Bruni
***************************************************************************