TECHNET Archives

May 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wRGVS-000Bj1C; Tue, 13 May 97 07:16 CDT
Old-Return-Path:
Date:
Tue, 13 May 1997 08:26:40 -0400 (EDT)
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/12641
TO:
From [log in to unmask] Tue May 13 13:
25:31 1997
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"koBDv3.0.5BI.bk5Up"@ipc>
Subject:
From:
Message-ID:
X-Loop:
>From bergdi Tue May 13 07:
17:04 1997
Parts/Attachments:
text/plain (16 lines)
I think by now all laminate suppliers have qualified their materials
to a CTI rating.  This rating will be on their UL card.  In the past,
not even UL or the laminate makers wanted anything to do with
this rating.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2