From:  Tuan300859

Currently, I have observed some boards with Tin Whiskers growth.  The
whiskers seem to grow from the Tin-lead pads(unusual).  The phenomenon is
occurred at only one side of the QFP180 component on the board.  Here are my
questions:

1.  What is/are the root cause(s) of the Tin Whisker?
2.  Are there experiments or tests that had been done?
3.  If no to both questions above,  Are there any literature that I can read
up to 
     help determine the root causes of the Whisker?

Thank you in advance 

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2