I'm trying to find data on the melting point (range) of a particular solder
alloy, Sn46 Pb46 Bi8. So far, the temperature ranges I came across are:
120 C to 167 C (IPC-J-STD-006)
163 C to 178 C (a Japanese company)
171 C to 186 C (a component foundry using this alloy - BGAs)
As you can see, I have conflicting stories. Can anyone tell me where I can get
good information? (By the way, I don't have a sample to test so don't suggest
it!)
Thanks again,
Jim Marsico
(516) 595-5879
[log in to unmask]
********************************
* ______ _ _ _____ *
* / ___ | | | | | _____ *
* / /___| | | | | | _____ *
* __/ ____ | | | | |______ *
* |____/ |_| |_| |________| *
* *
* SYSTEMS, INC. *
********************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|