Hi Folks!
Does anyone have any copper plating test results that they can share?
Specifically we are seeking to understand the range of physical properties
that are being seen. Tensile and elongation are of course the most common
attributes measured but we have interest in what other tests are commonly
employed and what values are common.(e.g. fatigue ductility, [ high and low
cycle], bulge testing etc.) Also there is interest in hardness and grain
structure. I will gladly summarize the information submitted back to all. I
am providing a form here that could serve as a template for the data.(If you
have additional information you would like to see please feel free to add
it) Thanks for considering this request and thanks in advance for you help.
Cheers!
J. Fjelstad
Copper type: Plated?... Yes No Type? Acid sulfate___ Pyrophosphate___
Other____
Bath
Additive Manufacture and type_________ (optional)
Rolled? ... Yes No Annealed? Yes No Alloyed?
Yes No
Metallurgical attributes (e.g size, orientation
etc.)_______________________
Tensile strength? Typical Value__________ Range of values
seen_________ Gauge length, width and thickness____
Test
conditions_________________________________________________
Elongation? Typical Value__________ Range of values
seen_________ Gauge length, width and thickness____
Test
conditions_________________________________________________
Fatigue dultitlty? Typical Value__________ Range of values
seen_________ Gauge length, width and thickness ____
Test
conditions_________________________________________________
Bulge test? Typical Value__________ Range of values
seen_________
Test
conditions_________________________________________________
Hardness? Typical Value__________ Range of values
seen_________
Test
conditions_________________________________________________
Other test(s)?? Typical Value__________ Range of values
seen_________
Test
conditions_________________________________________________
*************************************************************************
_/_/_/_/ /__ __/ / ____/ / ___/ / ___/ / ___/ / __ / / \
_/_/_/_/ / / / /___ /___ / / __ / / _ \
_/_/_/_/ / / / __/ / / / / __/ / / \ \ / ___ \
_/_/_/_/ /_/ /_____/ /____/ /____/ /_____/ /_/ \_\ /_/ \_\
...System Building Blocks for the Next Generation of Electronics
3099 Orchard Drive
San Jose, CA 95134
Phone 408 894-0700
Fax 408 894-0768
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|