Hello, Technetts:
We are experiencing a big problem with solder balls attaching to the bottom
of a through-hole connector during wave soldering.
We just switched to NoClean chemistry (Alpha NR300A2 water based flux).
Solder pallets are used during wave soldering. There is an opening for the
connector in the pallet and connector's plastic body (made from GM7001)
emerges into the solder pot during soldering.
I guess, we have had this problem before , but the solder balls were washed
away during the wash process.
The solder balls on the bottom of the connector are not acceptable per
customer spec.
Any suggestions would be appreciated.
Thank you, Stella Neyman
Lectron Products
ph. 248-608-7289
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|