TECHNET Archives

May 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wWuRM-000BjGC; Wed, 28 May 97 20:55 CDT
Encoding:
14 TEXT
Old-Return-Path:
Date:
Thu, 29 May 97 12:00:00 PDT
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/12981
TO:
Return-Path:
<TechNet-request>
X-Loop:
Resent-Message-ID:
<"bgyGr3.0.1uL.V8EZp"@ipc>
Subject:
From:
"Raich, Zoran" <[log in to unmask]>
>From bergdi Wed May 28 20:
56:00 1997
Message-ID:
From [log in to unmask] Thu May 29 09:
57:30 1997
X-Mailer:
Microsoft Mail V3.0
Parts/Attachments:
text/plain (26 lines)

Dear Technetters
We have some printed circuit boards with gold over nickel coating which   
are experiencing solderability problems, ie very poor wetting. I have   
heard that this may be due to nickel migration through the gold over   
time. The boards are approximately 6 Months old. Is there a particular   
shelf life for this type of coating before we need to dump the boards?.

Regards
Zoran Raich
Process Engineer
NetComm (Aus) Ltd
(+612) 9878 7394
[log in to unmask]  

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2