TECHNET Archives

May 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wUdSv-000BjAC; Thu, 22 May 97 14:23 CDT
Content-Type:
text/plain; charset=ISO-8859-1
Old-Return-Path:
Date:
Thu, 22 May 1997 15:31:54 -0500
MIME-version:
1.0
Precedence:
list
Resent-From:
>From bergdi Thu May 22 14:
24:26 1997
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/12899
TO:
Content-transfer-encoding:
quoted-printable
X-Loop:
Resent-Message-ID:
<"nxnsL.0.uYF.Br9Xp"@ipc>
Subject:
From:
From [log in to unmask] Fri May 23 08:
55:38 1997
Return-Path:
<TechNet-request>
X-Mailer:
TFS Gateway /220000000/221000897/221080605/221080779/
Message-Id:
Parts/Attachments:
text/plain (23 lines)
	Has anyone experienced dull, dark gray SMT solder joints after cleaning?
I am using a dishwasher and a neutralizer could these be the problems??

||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
    Dan Sadley                 
 [log in to unmask] 
3660 Quakerbridge rd.    
Trenton, NJ 08619         
(609) 587-9897 x-179     
 Fax (609) 587-1970        
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2