TECHNET Archives

May 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wUXPe-000Bj1C; Thu, 22 May 97 07:56 CDT
Old-Return-Path:
Date:
Thu, 22 May 97 06:05:13 PST
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
>From bergdi Thu May 22 07:
56:27 1997
X-Mailing-List:
<[log in to unmask]> archive/latest/12883
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"ChN_t.0.hbK.f94Xp"@ipc>
Subject:
From:
"sbryan" <[log in to unmask]>
Status:
O
X-Loop:
From [log in to unmask] Thu May 22 09:
46:55 1997
Message-Id:
Parts/Attachments:
text/plain (42 lines)
     
     Do the via plug after Hot Air Solder Leveling.  That should eliminate 
     the problem.


______________________________ Reply Separator _________________________________
Subject: Solder balls
Author:  [log in to unmask] at corp
Date:    5/21/97 12:34 PM


We're having problems with "solder balls" that are "resting in a nest". We 
have .025" via holes that are covered with L.P.I. soldermask. The mask is 
collapsing when going through our vertical hot air leveler and little 
"solder balls" are sitting just inside the holes. The solder balls are 
falling out at subsequent operations and in some cases are ending up between 
contact fingers that have .006" spacing between. The solder balls are 
creating a short at electrical test. They are easily removed but not easily 
detected before hand. Any ideas on what we can do to eliminate this problem?
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2