>From bergdi Wed May 14 03: |
22:25 1997 |
Sender: |
|
CC: |
|
Old-Return-Path: |
|
Date: |
Wed, 14 May 1997 09:31:50 +0100 |
Precedence: |
list |
Resent-From: |
|
Message-ID: |
|
MIME-Version: |
1.0 |
Status: |
O |
X-Mailing-List: |
|
TO: |
|
X-Status: |
|
Return-Path: |
<TechNet-request> |
X-Loop: |
|
Resent-Message-ID: |
<"_IY9W1.0.wg8.eONUp"@ipc> |
Content-Transfer-Encoding: |
7bit |
Content-Type: |
text/plain; charset=us-ascii |
From [log in to unmask] Mon May 19 09: |
18:34 1997 |
Subject: |
|
From: |
|
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0wRZJx-000Bj1C; Wed, 14 May 97 03:22 CDT |
X-Mailer: |
Mozilla 3.01Gold (X11; I; SunOS 5.5.1 sun4u) |
Organization: |
Fujitsu Telecommunications Europe Limited |
Resent-Sender: |
|
Parts/Attachments: |
|
|
James.
How are you currently breaking out the v-scored boards? Our
manufacturing guys use what is basically a powered, fixed, 'pizza style'
cutter. The panels are fed in, and the blades run down the score line
cleanly breaking out boards, thus minimizing any stress on the
components because the boards are never 'bent'.
I could find out more details on the machine if you're interested.
Regards,
Pete Court
[log in to unmask]
Fujitsu Telecommunications Europe Limited
> In the past
> when we have "V" scored small boards and then broken them away after
> population. We have had solder joints fracture and a large amount of
> rework. My question is, is there a distance that a component must be
> from the edge of a board when using "V" scoring to prevent damage to
> solder joints during board separation.
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|