Circuit Center in Dayton, Ohio says they can do it, but I have no idea what
their process is.
----------
From: Ed Cosper
To: [log in to unmask]
Subject: tetra-etch of Teflon
Date: Monday, April 07, 1997 12:41PM
I have been told recently that a board shop is producing teflon plated
thru circuit boards without using a tetra etch and using only a
permanganate.
Is this possible? I have always understood that unless you tetra etched
the material, you could not get good hole wall bond. Does anyone have
any information in this?
Ed Cosper
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|