> Gaby
>
> First, comparative tracking index has nothing to do with X-ray but is related
> to the relative resistance of solid electical insulating materials to
> tracking under moist conditions at voltages up to 600 volts. It is very
> seldome used in the US, but is a common for European requirement. Refer to
> International Electrochemical Commission (IEC Standard) Publication number
> 112. Document may be procured through ANSI in the United States> I do not
> have the numbers for many of the printed board materials, but the laminate
> suppliers, especially those who deal in Europe, can give you the tracking
> information on their materials.
>
> Phil Hinton
> Hinton "PWB" Engineering
>
> ***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 *
> ***************************************************************************
> * To subscribe/unsubscribe send a message <to: [log in to unmask]> *
> * with <subject: subscribe/unsubscribe> and no text in the body. *
> ***************************************************************************
> * If you are having a problem with the IPC TechNet forum please contact *
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
> ***************************************************************************
Thank you very much, Phil. I am sorry for my mistake concerning
the title of my request,I was sloppy while I wrote my correspondence
and put the same title on two different letters. Of course XRay has
nothing to do wih CTI.
Gaby
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|