In the past year, we have had problems with our tin tank not plating
properly. It has caused problems that resulted in annular ring failure
at the knee. I was wondering, can anyone provide inside into what to
check, and an reliable way to check the amount of brightners/wetting
agents in the bath. I am looking for tests (besides hull cell) that
doesn't cost a fortune.

If there is a way of testing the wetting agents on the Hull cell (full
bright), could someone please give some insight?

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2