Hello
We have used similar pitch components and the pad width is 12 mils, the
same as what you are using. So far we have not had any problems.
You can infact try using 10 mil pad width with mask inbetween pins (very
essential in case of 19.67 mil pitch components), which is quite good
enough for this package, incase that helps solving solder bridges.
thanks with regards
k.v.raj
____________________________________________________________
| |
| From*******************************************************|
| K.Varadaraj |
| CADET Automation Systems, No.1139, 26th A Main, 9th Block, |
| Jayanagar, Bangalore-560 069, India. |
|------------------------------------------------------------|
| Office : Residence |
|------------------------------------------------------------|
| Phone : 91 80 665 7215 : 91 80 529 6922 |
| Fax : 91 80 528 0101 : --- |
| Page : 91 80 9622733500 : 91 80 9622733600 |
| Email : [log in to unmask] : --- |
| ***********************************************************|
| |
| CADET --> Computer Aided Design Engineering and Test |
|<<------------- at your service since 1991 ------------->>|
|____________________________________________________________|
On Fri, 18 Apr 1997, Dan Ratcliff 813-530-8762 wrote:
> Hey y'all,
>
> We are having solder bridging problems on .5mm pitch SMD quad packages.
> We use an .012 wide pad. This results in .0077 spacing between pads
> I would like to know what pad sizes others are using as well as paste
> stencil opening size and thickness.
>
> Thanks,
>
> Dan Ratcliff
> Principal PCB Designer
> Paradyne Corporation
> Largo, FL
> 813-530-8762
> [log in to unmask]
>
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|