Hi,
We are using kraft paper (225 g/m2) and PACOFORM Pad (cellulosic-based,
thickness 1.524 mm) to control the heat up rate of our press.
Has sombody information about the specific heat J/kg.K and the heat
conductivity W/m.K of these materials.
Thanks a lot.
Bas van Zalk