          Hello,
          
          Does anyone have any experience with removing a high-density 
          (>100-pins) PTH connector that is both press-fit and soldered (not my 
          design)? So far, I came up with preheat/prebake @ 250 F for 1-4 hrs 
          and use a solder pot (i.e., Air-Vac), but I'm worried that I will 
          damage the through holes. 
          
          Regards,
          
          [log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2