We process the electro gold plating jobs (immersion type) in the following
manner,
RESIST STRIP->ALKALINE ETCH->TIN STRIP->PHOTO PRINT/DEVOLOP->GOLD PLATING
This process is follwed by us,as we maximise the panel size due to which
the tabs are generally not to the edges. please suggest if any other process/
route is possible.
thanks..
***************************************************************************