Hi David -
I suggest you contact Doug Pauls ([log in to unmask]), Tim Crawford (EMPF
317-655-3673), and Bill Kenyon (Global Centre for Process Change
302-652-4272) - all three are good sources for information on
alternative cleaning chemistries which may be of use to you. Good
Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________ Reply Separator _________________________________
Subject: Genesolv replacement
Author: [log in to unmask] at ccmgw1
Date: 4/15/97 1:21 PM
My name is David Fancher. I am the Quality Manager for a wire harness
assembly company called Precision Cable Mfg. Corp.
(http://www.precisioncable.com). Our primary use of solder is in wire
tinning and soldering. We do some PCB componernt mounting as well. My
company has been using Genesolv as a flux cleaner. I believe as of January
of this year, it is no longer available due to its harmful effects on the
ozone layer. I am looking for a comaprable replacement in terms of cleaning
ability.
We use Kester 1515 rosin flux, Kester "245" 63/37 core 50 solder (.031in. and
.050in. dia.), and 60/40 and 63/37 Kester Ultrapure bar solder. I would
appreciate any feedback anyone has regarding any recommendations of what
cleaner to use and where to get it.
My email address is [log in to unmask]
Thanks for your help
David Fancher
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|