text/plain (28 lines)

    \0
   TO:         I4235700 IBMMAIL   new address for ipc technet 25.6.96

   FROM:       DSTEWART EX2       D.Stewart        - Product Development Manager.

   DATE:       16 April 1997
   SUBJECT:    FAB: PLATING MYSTERY

    Do you use diazo film or silver halide? I remember a problem way
    back when the diazo was not fully exposed and began to wash out
    after a number of prints. It still looked the same but there were
    issues in printing as there was insufficient uv blocking to not
    expose the pattern.
    Dougal Stewart

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2