X400-Content-Type: |
P2-1984 (2) |
Old-Return-Path: |
<"/DD.MHS=BLAUROCJ(a)KLW (Blaurock, J.G.)/O=MHS (A) ARNHEM/"@akzo.nl> |
Date: |
Mon, 7 Apr 1997 12:19:00 +0200 |
From [log in to unmask] Mon Apr 7 09: |
54:46 1997 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
Priority: |
Urgent |
X400-MTS-Identifier: |
[/PRMD=AKZO/ADMD=400NET/C=NL/;F2DE483301B566D9] |
TO: |
|
X-Loop: |
|
X400-Originator: |
"/DD.MHS=BLAUROCJ(a)KLW (Blaurock, J.G.)/O=MHS (A) ARNHEM/"@akzo.nl |
X-Mailing-List: |
|
X400-Recipients: |
|
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0wEBGm-000BipC; Mon, 7 Apr 97 05:03 CDT |
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"JLtd03.0.344.gPCIp"@ipc> |
Subject: |
|
From: |
"/DD.MHS=BLAUROCJ(a)KLW (Blaurock, J.G.)/O=MHS (A) ARNHEM/"@akzo.nl |
Message-ID: |
<"F2DE483301B566D9*/DD.MHS=BLAUROCJ(a)KLW (Blaurock, J.G.)/O=MHS (A) ARNHEM/PRMD=AKZO/ADMD=400NET/C=NL/"@MHS> |
X400-Received: |
by /PRMD=surf/ADMD=400net/C=nl/; Relayed;
Mon, 7 Apr 1997 11:56:13 +0200
by mta relay.surfnet.nl in /PRMD=surf/ADMD=400net/C=nl/;
Relayed; Mon, 7 Apr 1997 11:56:13 +0200
by /PRMD=AKZO/ADMD=400NET/C=NL/; Relayed;
Mon, 7 Apr 1997 12:19:00 +0200 |
Importance: |
High |
Alternate-Recipient: |
Allowed |
Parts/Attachments: |
|
|
Ladies & Gentlemen:
I am currently setting-up a lab in good old Europe for inspecting and
testing thin copper-clad linear laminates. My problem is that I haven't
been able to find a vendor for arc resistance equipment, neither in
Europe nor in the US. Beckman Instruments, mentioned in IPC-TM-650 2.5.2,
couldn't be reached.
Who can help?
Regards,
J. Blaurock
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|