TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wDCHb-000BilC; Fri, 4 Apr 97 10:56 CST
Old-Return-Path:
Date:
Fri, 04 Apr 97 10:21:30 MST
From [log in to unmask] Fri Apr 4 11:
08:03 1997
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/11714
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"skkzT2.0.9vA.fAJHp"@ipc>
Subject:
From:
Precedence:
list
X-Loop:
Cc:
Donald_DesCamps@smtpr, Brett_Sanderson@smtpr
Message-Id:
Parts/Attachments:
text/plain (33 lines)
     Hello,
        What methods are available for testing the adhesion of dry film 
     resist on inner layers? 
        Has anyone used ASTM D4541 "Pull-Off Strength of Coatings Using 
     Portable Adhesion Testers"? A fixture is attached to the coating using 
     epoxy. The fixture is pulled away and the force required to do so is 
     measured.
     Thanks
     Rich
------------------------------------------------------------------
     Richard Olsen                Telephone (602)-232-9154
     Continental Circuits Corp.   Main      (602)-268-3461
     3502 East Roeser Road        Fax       (602)-268-0208
     Phoenix Arizona              Pager     (602)-310-6245
     85040-2905                   Internet  [log in to unmask]
     USA                    I make circuit boards,what do you do?
------------------------------------------------------------------
     
     
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2