TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=us-ascii
From [log in to unmask] Thu Apr 17 13:
23:41 1997
References:
Date:
Thu, 17 Apr 1997 12:16:39 -0400
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/12078
TO:
Return-Path:
<TechNet-request>
X-Loop:
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wHteC-000BkuC; Thu, 17 Apr 97 11:02 CDT
Resent-Message-ID:
<"nABSa3.0.4JJ.kcaLp"@ipc>
Subject:
From:
Mike Masters <[log in to unmask]>
Old-Return-Path:
In-Reply-To:
"Dan H. Arnold" <[log in to unmask]> "TBGA's on "big boards"" (Apr 17, 8:59am)
X-Mailer:
Z-Mail 4.0.1 (4.0.1 Apr 9 1996)
Message-Id:
<970417121605.ZM8751@msaipc>
Parts/Attachments:
text/plain (37 lines)

I have a bare PCB with 1 via pad missing on one side of the PCB.  This is a 
multilayer PCB.  After assembly some pass test while others did not.  This is 
how the problem was discovered.  The problem is that several hundred assemblies 
have been produced and are still in-house.  I plan to temperature cycle the 
assemblies to insure connection with the innerlayers.

Has anyone experienced this problem and if so how was it verified reliability 
wise as good product.  If there is not an effective test method of course all 
product will be scraped and sent back to the supplier for reimbursement.

Any ideas?  Any test methods for reliability?

Mike

-- 

Mike Masters
QA Materials Engineering section
Office: (919) 479-3771
FAX:    (919) 479-3328
Internet:  [log in to unmask]



***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2