Ladies & Gentlemen:
I am currently setting-up a lab in good old Europe for inspecting and
testing thin copper-clad linear laminates. My problem is that I haven't
been able to find a vendor for arc resistance equipment, neither in
Europe nor in the US. Beckman Instruments, mentioned in IPC-TM-650 2.5.2,
couldn't be reached.
Who can help?
Regards,
J. Blaurock
***************************************************************************