Tenting .020 holes with a liquid mask is pushing the envelope a
bit. Normally I recommend customers not to exceed .018 holes.
Holes larger than .018 normally use one of the various dry film
masks.
I will contact you off line to discuss options.
Bob Metcalf
Morton Electronic Materials
>>> "LANmark Circuits,Inc." <[log in to unmask]>
04/30/97 11:14am >>>
We've been battling a problem with LPI covering (tenting) larger
vias (>.020).
There is a tendency for the mask to lift around these holes,
particularly in
ground planes, at HAL. We've been drying the panels after scrub
in a heated
board dryer and a quick bake in the oven. We are using
Dynachem Epic mask.
Any input would be appreciated.
John Gordon
LANmark Circuits
LANmark Circuits,Inc.
400 Crown Point Circle
Grass Valley,Ca. 95945
(916)272-7280(voice)
(916)272-7017(fax)
***************************************************************************
* TechNet mail list is provided as a service by IPC using
SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to:
[log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body.
*
***************************************************************************
* If you are having a problem with the IPC TechNet forum please
contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at
[log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|