> hi all,
>
> it would be appreciated if someone could share information on
> drilling parameters (speeds and feeds)for best results
> (as less smear in hole as possible) , on polyimide 6 layers flex , with
> 2 fr4 stiffiners.
> most of the holes are 1 MM diameter,
>
> thanks
>
> Yisrael Leshman
> [log in to unmask]
***************************************************************************