Hi all,
We have a minor problem at wave soldering shields on 8-layer FR-4.
The problem is that we need a very long dwell time (6-8secs) to get the
solder to wet all around the shield, it's very critical because it has
to be a tight joint. This leads to a high temperature at topside of the
board at soldering, and inside the shields we have SMD-ICs which joints
reach an temperature to about 209 degC.
But then if i raise the preheating temperature and lower the dwell time,
the shields won't get this tight joint and misses corners and some
long-sides, this cost some to rework.
Some additional info: Seho wave solderer, NO-CLEAN flux, We put some
extra flux around the shield, we use a chip-wave to get better wetting.
Anyone have more ideas?
/Jan Merstrand
Wave Soldering Technician
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|