TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wLynZ-000BiqC; Mon, 28 Apr 97 17:21 CDT
Encoding:
34 Text
From [log in to unmask] Tue Apr 29 10:
53:38 1997
Old-Return-Path:
Date:
Mon, 28 Apr 97 17:16:44 cst
Precedence:
list
Resent-From:
Cc:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/12292
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"mQr_k.0.K_7.eBIPp"@ipc>
Subject:
From:
"ddhillma" <[log in to unmask]>
X-Loop:
Resent-Sender:
TechNet-request [log in to unmask]
Message-Id:
Parts/Attachments:
text/plain (47 lines)
     Hi TechNet -
     
     The IPC Microsectioning committee put out a poster that contains 
     several common board defects in a cross sectional view. Contact Mike 
     Buetow at IPC for more info.
     
     
     Dave Hillman
     Rockwell Collins
     [log in to unmask]


______________________________ Reply Separator _________________________________
Subject: Cross Section Defects
Author:  [log in to unmask] at ccmgw1
Date:    4/28/97 2:28 PM


     Many years back DEC had posters of some common defects found in cross 
     section.  My technicians have been asking if there are any newer 
     posters available in the industry?  I have contacted Struers and they 
     do not believe they have any or know of any available.  Any 
     suggestions?
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2