Boyd Anderson writes
>Does anyone have any experience using magnesium hydroxide as a neutrializer
>prior to adding DTC in a waste water treatment application?
>
>Will the DTC also remove the magnesium, thus using more DTC than would
>normally be required?
>
>We are using mag. because it gives us a much heavier partical that settles
>faster. If anyone has found something else that makes a heavier sludge
>with DTC would you provide some feedback?
>
>Thanks,
>
>B.A.
Hi Boyd,
We use Lime (Calcium Hydroxide) as a neutraliser and it settles very
well. You have to keep it in a slurry by constant stirring and pumping
around the dosing circuit to stop it settling out and clogging up the
system. We also add a flocculating agent just before clarifying.
Another key element is to acidify the effluent to crack the ions before
neutralisation.
Can you please enlighten me as to what DTC is?
--
Paul Gould
[log in to unmask]
Isle of Wight,UK
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************