TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=us-ascii
Old-Return-Path:
Date:
Tue, 22 Apr 1997 11:56:29 -0500
Precedence:
list
Reply-To:
Resent-Sender:
TechNet-request [log in to unmask]
Content-Transfer-Encoding:
7bit
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/12128
TO:
X-Status:
Return-Path:
<TechNet-request>
X-Loop:
Resent-From:
Cc:
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wJneG-000BrDC; Tue, 22 Apr 97 17:02 CDT
Resent-Message-ID:
<"wf1I9.0.3ID.6MJNp"@ipc>
Subject:
From:
X-Mailer:
Mozilla 3.0C (WinNT; I)
From [log in to unmask] Wed Apr 23 17:
22:58 1997
Organization:
3M Columbia
Message-Id:
Parts/Attachments:
text/plain (29 lines)
Hello,

I work with an area that inspects flex circuitry.  The product is
gold or tin-plated copper circuitry on a polyimid substrate.  The
inspection is done with microscopes at stations which accomodate
roll-to-roll processing.  Many of our inspectors complain of the
glare from the product when inspecting the product with top lighting
from the scopes - especially when inspecting with top lighting several
hours a day.

Has anyone else dealt successfully with this issue?  I'd like to
improve the inspection conditions, if at all possible.  Any ideas
would be appreciated.
-- 
Mark M. Lettang       Opinions expressed herein are my own and may
[log in to unmask]     not represent those of my employer.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2