TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wC4Wr-000BioC; Tue, 1 Apr 97 08:27 CST
Old-Return-Path:
Date:
Tue, 1 Apr 1997 09:37:03 -0500 (EST)
Precedence:
list
Resent-From:
Message-ID:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/11621
From [log in to unmask] Tue Apr 1 09:
06:14 1997
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"YBm2u.0.71N.3jHGp"@ipc>
Subject:
From:
X-Loop:
Resent-Sender:
TechNet-request [log in to unmask]
Parts/Attachments:
text/plain (23 lines)
One of the biggest drawback for shrink wrap is usualy ESD concerns.
ESD is not too bad for fabricated boards but companies do not like to
see this stuff coming into their factories.  If it's assembled boards, then
this is a no no....I think there are some materials like poly which 
do not build up a charge, but this is usualy vaccum formed and to the
correct configuration of the assembled board.`
I have shrink wrapped assembled boards to keep components in place
before wave soldering and what happened was the material formed around
components, tough to get off, and this was before ESD became known as
a problem. Wouldn't do this anymore.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2