TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wGx1n-000BilC; Mon, 14 Apr 97 20:27 CDT
Old-Return-Path:
Date:
Mon, 14 Apr 1997 21:37:11 -0400 (EDT)
Precedence:
list
Resent-From:
Message-ID:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/11946
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"3MPdb1.0.QkC.wbjKp"@ipc>
Subject:
From:
From [log in to unmask] Tue Apr 15 08:
56:14 1997
X-Loop:
Resent-Sender:
TechNet-request [log in to unmask]
Parts/Attachments:
text/plain (29 lines)
All

I am looking for a supplier that can furnish good quality boards made with
cyanate ester and containing two copper-Invar-copper planes that serve as
power and ground.
The boards must be able to qualify to IPC-RB-276 Class 3 which imposes a
horizontal microsection on any clearance holes in the CIC and no radial
cracks are allowed that decrease spacing between the hole barrel and the
planes.  The interconnections between the CIC layers and the hole barrel must
also be to RB-276 and pass 100 cycles between -65and +170C without
separation.

May reply to: Technet or [log in to unmask] or 520-745-1013 which is also a FAX

Phil Hinton 
Hinton "PWB" Engineering 

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2