TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wGhJs-000BilC; Mon, 14 Apr 97 03:41 CDT
Old-Return-Path:
From [log in to unmask] Mon Apr 14 15:
51:34 1997
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/11927
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"aUFSG2.0.oy6.RsUKp"@ipc>
Subject:
From:
Karl Ring <[log in to unmask]>
Message-ID:
X-Loop:
Date:
Mon, 14 Apr 1997 04:49:56 -0400
Parts/Attachments:
text/plain (25 lines)
Hello all

IPC Testmethod Number 2.3.25 (Date 2/88)  Resistivity of Solvent Extract
seems to have an error. 
Nr. 2.3.25 requires 100ml of wash solutions for each 250mm2 of the board
MIL-STD-2000A requires 1.55ml for each cm2 (also MIL-P-28809 10ml/in2)

i think IPC should reqire 100ml at 6451.6mm2
Is this correct?

Karl Ring
ZVE - Germany

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2