Kirkendall voids are voids that develop as two metals diffuse into each
other and the term is predominently used to describe wire bond failure
mechanisms.
Check out:
http://www.eccb.org/pbps/tg/wirebond.htm
ain't technology wonderful???
Dave Rooke
Circo Craft - Pointe Claire
_________________________
>I've been stumped by a phrase which one of our Japanese customers used in a
>correspondence with us recently. The phrase is "Kirkendall void" and the
>context it was used in is:
>
>"There are some electrode that are gold plated and also solder welded. If
>there is gold at solder welded part, Kirkendall void may be formedm
>resulting pealing."
>
>
>It is possible that the CCA they were looking at has gold plated leads
>installed on gold plated PWBs and reflowed with Sn63Pb37 solderpaste.
>
>Any help would be gratefully accepted,
>
>
>Regards,
>
>
>Phillip A. Bavaro
>Senior Manufacturing Engineer
>[log in to unmask]
>(619) 658-2542
>
>
>***************************************************************************
>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>***************************************************************************
>* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
>* with <subject: subscribe/unsubscribe> and no text in the body. *
>***************************************************************************
>* If you are having a problem with the IPC TechNet forum please contact *
>* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
>***************************************************************************
>
>
>
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************