Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0wCS5f-000BjBC; Wed, 2 Apr 97 09:36 CST |
Content-Type: |
text/plain; charset="us-ascii" |
Old-Return-Path: |
|
Date: |
Wed, 02 Apr 1997 16:00:12 -0500 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
X-Sender: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Loop: |
|
Resent-Message-ID: |
<"MAjRV3.0.sAD.DqdGp"@ipc> |
Subject: |
|
From: |
|
From [log in to unmask] Wed Apr 2 09: |
50:16 1997 |
Mime-Version: |
1.0 |
X-Mailer: |
Windows Eudora Light Version 1.5.4 (16) |
Message-Id: |
|
Parts/Attachments: |
|
|
Dave,
This figure is for an inert atmosphere - under e.g. flux it will be different
e.g. Klein Wassink in "Soldering in electronics" shows figures between 0.41 and
0.33 N/m for solder under colophony flux with activations between 0 and 1%
respectively!
In our own experiments we measured a value of 0.426 N/m for multicore NA
colophony at 235C (D.C.Whalley & P.P.Conway "The globule block wetting
balance test",
Transactions of the ASME: Journal of Electronic Packaging, Vol.118:134-141,
No. 3,
September 1996).
David Whalley
Loughborough University
At 07:01 31/03/97 cst, you wrote:
> Hi TechNet!
>
> The surface tension for alloy Sn60/Pb40 at 500 C is 472 mN/meter. The
> source of the value is Tin Research Institute data.
>
>
> Dave Hillman
> Rockwell Collins
> [log in to unmask]
>
>
>______________________________ Reply Separator
_________________________________
>Subject: Surface tension of molten Pb/Sn
>Author: [log in to unmask] at ccmgw1
>Date: 3/30/97 5:06 AM
>
>
> Hello,
>
> I need the surface tension of the eutectic solder Pb/Sn.
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|