We've experienced a problem with OSP coated product
after the product has been shrink-wrapped and sits in
storage for a period of days. Dark blueish-black spots
appear on the surface of many pads and annular
rings. We have no idea what causes this. We
refer to it as the "fungus" since it closely resembles
what you might see on an orange after a month in your
refrigerator.
Has anyone had any experience with this? Our OSP
provider has no idea what it could be. Our
experimentation has yielded no info. We haven't been
able to consistantly reproduce the problem.