I have a serious problem on some of the board that stucked in the store.
All of them is at least 2 years.
When I wave-soldered the bare board, it has a lot of blow-holes, solder
balls, pin-holes.
Anyway, I try to purge all of them, but there are 6000 pieces in the Store.
I try to bake at at 100 deg. C for 4 hours. Too bad, it doesn't work.
I try to bake for any 4 hours just before wave-soldering. The result is
terrible. Not even a slight Help !!!
Can anybody give me some advises what should I do ???
Thanks in Advance
Poh ..
***************************************************************************