     Hi TechNet!
     
     There was an enormous amount of data presented at the IPC Expo 
     Alternative Finishes session in San Jose. Take a look at the Expo 
     proceedings for more information on Pd,Au,Ag, OSPs and other finishes 
     which the industry is currently looking at from various angles.
     
     
     Dave Hillman
     Rockwell Collins
     [log in to unmask]


______________________________ Reply Separator _________________________________
Subject: ASSY:ALTERNATIVES TO HASL
Author:  [log in to unmask] at ccmgw1
Date:    3/27/97 3:25 PM


 DOES ANYONE KNOW ABOUT THE ADVANTAGES / DISADVANTAGES OF USING NiPd AS AN=20=
ALTERNATIVE TO HASL. I'M LOOKING FOR A FLATTER PAD SURFACE AND HIGHER YEILD=
 FROM MY FINE PITCH.
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2