>From: frp
>Sent: Monday, 24 March, 1997 19:00
>To: [log in to unmask]
>Subject: Interconnection Resistance, Multilayer Printed Wiring.
>
>Hi everybody,
>I have a problem with the test methode number 2.5.12 of the IPC-TM-650.
>This test methode tells you to use test coupon "G" as discribed in part
>5.8.4 of the IPC-TM-650.
>It also tells you which holes you should use to perform the test on.
>But if you then look to test coupon "G" the holes which are mentioned
>are not connected. How is it than possible to measure the
>interconnection resistance between those holes?
>Thanks in advance.
>Frank Petit
>
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|