     Hi Mike -
     
     Look over "Solder Mechanics: A State of The Art Assessment", by Frear, 
     Jones,Kinsman, ISBN # 0-87339-166-7. Chapter 2 on Physical Metallurgy 
     of solder-substrate reactions has great alloy summaries and a very 
     complete listing of references that may be of interest.
     
     
     Dave Hillman
     Rockwell Collins
     [log in to unmask]


______________________________ Reply Separator _________________________________
Subject: Mechanical Properties: Intermetallic Thickness!
Author:  [log in to unmask] at ccmgw1
Date:    3/21/97 12:07 PM


     
Related question on mechanical properties!
     
Are there any publications out there documenting  the adverse impact(s) of 
excessive intermetalic growth of  Eutectic Solder (Not Gold Embrittlement 
just regular Cu3Sn and  Cu6Sn5)?
     
Thanks
     
     
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2