Altarnatives to HASL are:

A. Metal coatings

1. Immersion Gold over the electroless nickel (Aurotech, Ronamerse SMT)
2. Immesion Silver (Alpha Level)
3. Electroless Palladium (Pallatect, Pallamerse SMT)
4. Immersion tin (APT 884, Tinposit)

B. Organic coatings (benzimidazole or imidazole based compounds,  often couple
d with co-deposited copper)

1. Shercoat (Atotech)
2. Entek Plus (Enthone)
3. Ronacoat (LeaRonal)
4. MecSeal (Mec)
5. M- Coat Plus (MacDermid)
6. Glicoat - F1, E3 (Shikoku)

Regards

Michael Pavlov

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2