[correction to my previus mail]

Hi friends,
In order to  make high produceability in the soldering process of boards, surface mounted,
it is necessary to prepare the gold plated components before assembly. This is
stated in ANSI/J-STD-001, which does not allow any gold at all on the component legs.

Is it, anyway, possible to specify a limit of gold thickness on the comp. connections, below which
it is not necessary to extract the gold before soldering? Does anyone have a opinion
about that?

Sven-Eric Backstrom
Ericsson Saab Avionics
Sweden


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2